Carbon fiber infusion kit and more questions


Author
Message
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
Hello guys after Warren help i decided to buy resin infusion kit from easycomposites.

im interested if i add to my buying list - Through-Bag Connector - that mean i can do both ways my work with this end i can put it and do vacuuming and taking him of i can do infusion so 2 works? am i correct?

Also Can you please reply dear moderator what best price for this everything you can do delivered to london?



also like i understood things like: Flash Breakers release tape into kit infusion?


And about material i saw carbon fiber  15mm Spread-Tow- what i see its very big waves patter i mean almost like zonda pagani or i mistaken?

Thank you very much.