Working carbon fibre


Author
Message
coolukey
coolukey
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Awaiting Activation
Posts: 3, Visits: 8
If I want to reduce a length of carbon fibre solid rod in the middle, with a gentle taper from each end, will it affect it's strength or properties at all ? Or will it fracture in any way ?
Replies
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Coolukey,

What ezsailor is saying seems about right; thanks for your input. If you taper the rod in the middle then you'll create an inherent point for a fracture to start and so it will have more impact on the overall strength than just being proportional to the reduction in cross section. If you engineer some 'margin' in to the rod in the first place then this doesn't necessarily have to mean that you can't do it just that the penalty for breaking the continuity of fibres will be more than you might expect. ezsailors advice for machining is helpful; you will find that turning us a really awkward way to work with a pultrusion because you're going straight across the grain making splintering/fracturing more likely.

As for the safety; follow sensible precautions always when cutting carbon fibre; wear a mask and clean up/extract the dust.

All the best, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
coolukey
coolukey
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Awaiting Activation
Posts: 3, Visits: 8
Hi

Thank you for your comments. My main concern was, that however I reduce it, would it create a weak area as I was cutting across the fibres. The taper would not meet in the middle in the form of an angle, more of a gentle curved shape. It's use, when made, will require it to flex and return as best and repeatedly as possible. The thickness will be reduced from 6mm to about 3.5mm to 4mm. I guess I'll have to experiment somewhat. I bought a metre length of 6mm and will be cutting it down to 160/200mm pieces. I will have to reduce it by abrasion as I have no other means available.

Thanks again for your much appreciated input.

ps.   Is it possible to have a piece made to this shape? If so will it be costly?