posted 4 Years Ago
ANSWER
HOT
Topic Details
c
Group: Forum Members
Posts: 34,
Visits: 2.7K
Hi guys, is the zyvax release agent good on epoxy molds. Their blurb talks about it being developed for polyester environments,
ie Formulated to control physical and chemical factors in
polyester-molding environments.
Cheers...Chris
Reply
Like
7
Hanaldo
Hanaldo
posted 4 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Yes, works perfectly with all resin systems, I use it every day
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search