Hi, first of all, big thumbs up for the easy composites team. Great tech. support, youtube, wepshop etc. you got me into trying carbon fibre. Well done!

I'm new to carbon fibre and just wanted to get some tips and tricks from more experienced doers. I have vacum bagging equipment and have been doing a few test just with plates on glass to get a grip on laying up wet and mixing epoxy, vacum, bagging and so on, I did one intake tube (not one a really need) just to learn and see how difficult it is and how to not do. I have a 3D printer so I will print molds and coat them with XCR epoxy+relese, the same way I did with this test tube mold.

What I learned was that you cannot do anyting with the inside of the tube if I put the bottom half on the table and then the internal vacum tube through. And thats ofcourse totally obvious after you have done it once Smile, could only get the peelply on one half as I needed the CF parts to overlap and so on and so on...




But to the real project, this is what I want to build. A modular CF intake, that are in three parts + aluminum flange + throttlebody flange in alu. Three parts so I can make different lengths of runners and different size and shape of plenum depending on the case.

I was planning to bond with structural adhesive as you see with over lap of 7-10mm. Planned thicknes is now 2.5mm, is that overkill?



Any comments and thougths on bonding points and thicknes of the part?

When split in this way its also more easy to wet lay parts. maybe I'll try infusion later.

Anyone aware of 3D printer filament that can take the prepreg heating process?

/André


Edited 3 Years Ago by norrback
Reply
André Norrback
A
Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)
Group: Forum Members
Posts: 4, Visits: 99
hi.

ok, thanks. I think I go with about 1,5mm for runners and about 2mm for the rest then it will be enough.

Yeah, I had a hard time having peeply on both halves in my first trial, but I think I can get it done next time. I put the internal tube last, after I have put halves together and have peelply applied, then I put the inner tube through. Should be doable.

when you say key the surface, what process is that?

OK, so even if I have no brether that takes up exess through perforated release I could squeeze out too much from the reinforcement to the bag it self?

No thoughts on 3D printing filament that can take pre-preg owen temps?

Thanks again for your input.

/André
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
norrback - 3 Years Ago
Warren (Staff) - 3 Years Ago
norrback - 3 Years Ago
Warren (Staff) - 3 Years Ago
norrback - 3 Years Ago
norrback - 3 Years Ago
Warren (Staff) - 3 Years Ago
Threedprof - 3 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search