Hi, first of all, big thumbs up for the easy composites team. Great tech. support, youtube, wepshop etc. you got me into trying carbon fibre. Well done!

I'm new to carbon fibre and just wanted to get some tips and tricks from more experienced doers. I have vacum bagging equipment and have been doing a few test just with plates on glass to get a grip on laying up wet and mixing epoxy, vacum, bagging and so on, I did one intake tube (not one a really need) just to learn and see how difficult it is and how to not do. I have a 3D printer so I will print molds and coat them with XCR epoxy+relese, the same way I did with this test tube mold.

What I learned was that you cannot do anyting with the inside of the tube if I put the bottom half on the table and then the internal vacum tube through. And thats ofcourse totally obvious after you have done it once Smile, could only get the peelply on one half as I needed the CF parts to overlap and so on and so on...




But to the real project, this is what I want to build. A modular CF intake, that are in three parts + aluminum flange + throttlebody flange in alu. Three parts so I can make different lengths of runners and different size and shape of plenum depending on the case.

I was planning to bond with structural adhesive as you see with over lap of 7-10mm. Planned thicknes is now 2.5mm, is that overkill?



Any comments and thougths on bonding points and thicknes of the part?

When split in this way its also more easy to wet lay parts. maybe I'll try infusion later.

Anyone aware of 3D printer filament that can take the prepreg heating process?

/André


Edited 3 Years Ago by norrback
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
For NA 1mm is plenty.  You want thicker for boosted applications but its a bit more complex as shape will determine thickness etc. 

If you are struggling to get the bagging stack in place with the fabric overlap, you may struggle to add extra layers hence why you aren't using peel ply now?

You can certainly add extra layers internally afterwards just ensure you key the surface and thoroughly clean before you laminate.  That can be useful if you struggle with the joins as you can wet lay carbon tape over the joins.

Vacuum bagging in general, 20% vac is the starting point.  You can adjust it up and down to get the finish you want.  Too much extra vacuum will squeeze out too much resin leaving the part dry.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
norrback - 3 Years Ago
Warren (Staff) - 3 Years Ago
norrback - 3 Years Ago
Warren (Staff) - 3 Years Ago