	Group: Administrators 	        
    Posts: 2.5K, 
    Visits: 8.5K 
    
 
          
		     | 
				                       
                 
                
                    
			            I would check the thickness of your gel and also stability of the mould.  If the gel is too thick and/or the mould moves quite a bit during curing etc then it could cause issues.
  Also I see a bit of print, perhaps check you leave it long enough to cure before demoulding as that can cause print as well as making it harder to demould, which may make cracks that become visible later in the cure cycle.                
			            
  				
			            Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant                     
                     
                                            
                         
                    
                  
             |