Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Will definitely be hard to hide the step, on something the size of a bonnet you will need a LOT of resin/clear coat to bury the overlap thickness so it isn't noticeable.
I wouldn't do it. Either practice handling the carbon so you can do a neat butt joint (an Olfa style cutter is your friend here), or look for some 1.5m wide carbon.
|