Thanks!
The hardener says 7 days but the resin says 24h, i'm not sure what this means
The product description made me a bit worried thu -
YD-114
is generally used in solvent free coating, floor coating,
trowelling application, crack injection systems, adhesives,
decoupage system, and high solids or low VOC industrial
coatings.
No wording on fabric lamination, do you know this product? is it suitable?Either way, here is the timeline process:
From lamination to cut - 3 days
from gluing to peeling - 4 days
Room temp is around 25 day and 20 night
So it should have been fine i guess
I've tested gel super glues

Your advice about gluing epoxy is extremely important for me and very helpful!
Can you recommend a glue that will be suitable for the job?The thing that i'm suspecting is the mixing ratio - it says 3/1 but the orders i got from the store are for 100g resin/ 60g hardener