Hi, I have been asked to make an item in carbon but the guy already has the mould. However, the mould is made from polyester so how can i protect his mould?


Reply
jeffrey bres
j
Supreme Being (505 reputation)Supreme Being (505 reputation)Supreme Being (505 reputation)Supreme Being (505 reputation)Supreme Being (505 reputation)Supreme Being (505 reputation)Supreme Being (505 reputation)Supreme Being (505 reputation)Supreme Being (505 reputation)
Group: Forum Members
Posts: 42, Visits: 469
My moulds are polyester gelcoat with vinilester tooling resin from unimould system of ec.

I use 8 layers of easylease and 2x wax on top on the first pull.   Then i just wax it every pull.

Im using epoxy resin to make my parts.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search