making polyurethane mold for boat hull


Author
Message
romain patanchon
romain patanchon
Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)Junior Member (24 reputation)
Group: Forum Members
Posts: 1, Visits: 6
Good morning all,
As part of a student project I have to make an infusion flax fiber boat hull.
Having a fairly small budget, I have to make my mold myself (4 large molds 2500mm * 1000mm * 600mm).

I chose to make a rigid polyurethane foam mold that I would come to cut in order to have my shape.
However, I don't know what product to use next to waterproof my mold and obtain a smooth surface effect.
I saw that the S120 (https://www.easycomposites.co.uk/s120-advanced-board-sealer) might be suitable what do you think? what about duratec 707-002 (https://www.castrocompositesshop.com/fr/appr%C3%AAts/1557-1323-duratec-707-002-appr%C3%AAt-polyester-gris-fonc%C3%A9 -compatible-% C3% A9poxy.html # / 403-weight-495_kg_100_g_de_pmec)?
What products do you use to make your molds? Have you ever made polyurethane molds?

I also thought of putting film of stabilizer for model making oracover type but I do not know if it adheres well to the surface.

In any case, thank you for your advice and I hope to have feedback from youWink

**Sorry for the traduction I am french and english is not my best asset.
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Unless its a high density model board as opposed to a foam, chances are the S120 will not have the filling abilities to fill the surface pores on a typical foam.  Ideally a thin scrim of woven glass and a good quality coating epoxy,  such as our XCR Coating resin, should give you a usable surface to work from.  It should be slightly more durable than Pattern Coat Primer and other pattern coating materials as they are generally designed for a single use for mould making. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search