I've been vacuum-bagging carbon fiber panels and have noticed that the side of our panel curing on our glass table comes out with streaks. The streaks don't come off when wiped down with acetone. I think this probably has to do with the surface we're laying up on. To aid in release, we apply three layers of Partall Wax to our glass worktable and let each layer cure for 5 minutes. Should we let the partall wax cure for longer? Are we not buffing well enough? Would a layer of PVA over the wax help minimize streaks? I'd appreciate any advice. 
Reply
ArturK
ArturK
Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)
Group: Forum Members
Posts: 19, Visits: 53
vniebles - 2/17/2021 5:50:13 PM
I've been vacuum-bagging carbon fiber panels and have noticed that the side of our panel curing on our glass table comes out with streaks. The streaks don't come off when wiped down with acetone. I think this probably has to do with the surface we're laying up on. To aid in release, we apply three layers of Partall Wax to our glass worktable and let each layer cure for 5 minutes. Should we let the partall wax cure for longer? Are we not buffing well enough? Would a layer of PVA over the wax help minimize streaks? I'd appreciate any advice. 


Use NC 770 release agent or Easy-Lease from Easy Composites and that will resolve the problem with your carbon fiber sheets manufacturing.


Carbon fiber sheets and composites .
www.dexcraft.com
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search