Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
You normally cut it like any composite cured part then finish off by trimming off the fluff with a sharp scalpel or similar fine blade.
If the design allows, stop the kevlar a few mm from the edge of the part, filling in with carbon or other laminates. That way you don't have to cut the kevlar at all once cured.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|