Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Are you using pre-preg or wet-lay? The non-perforated release film you see in that bike video is really for pre-preg only, where the resin content is already controlled. If you're doing wet-lay, you wouldn't use that film because as you say, you can't remove excess resin.
You could use a perforated release film though? Would have the same benefits that they used it for in the bike vid, but would allow some resin bleed.
|