Hi guys I've decided that I need to move from Qualatex balloons to a silicone bladder.
I've got Smooth On rebound coming just because there isn't much available in NZ at the moment.
Its a three part mold and I've built fiber glass shells to go in the mold parts to correctly size the bladder.

I will mess around with some trials but I'm was a little bit confused about the right time to do second coats and joins last time I did this.
I was using dragon skin then and it seemed to go from runny to tack free without a good tack period to second coats and a complex join.

One thing I did learn last time is that acetic cure tube silicone sticks like s*** to a blanket with smooth on silicone for fixing seam flaws.
The idea is to make a thin patch with the smooth on silicone and then glue it on with the cheap tube silicone.

Any pointers would be massively appreciated...Chris
Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Silicone will bond pretty well to itself if it is fresh. The fresher it is, the better it will bond. So I generally do the next layer as soon as the previous layer is firm enough to not disturb it when you apply the next layer.
chriscnf
c
Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)
Group: Forum Members
Posts: 34, Visits: 2.7K
Hanaldo - 1/10/2021 10:09:48 AM
Silicone will bond pretty well to itself if it is fresh. The fresher it is, the better it will bond. So I generally do the next layer as soon as the previous layer is firm enough to not disturb it when you apply the next layer.

In that case this should  a breeze...cheers Hanaldo...

chriscnf
c
Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)
Group: Forum Members
Posts: 34, Visits: 2.7K
chriscnf - 1/10/2021 5:25:03 PM
Hanaldo - 1/10/2021 10:09:48 AM
Silicone will bond pretty well to itself if it is fresh. The fresher it is, the better it will bond. So I generally do the next layer as soon as the previous layer is firm enough to not disturb it when you apply the next layer.

In that case this should  a breeze...cheers Hanaldo...

Not quite a breeze but got a good result. I'm thinking about a release agent to help with getting the bladder out of the close mold and to extend its life.
The areas inside the product that I need to adhere epoxy to  are protected by peel ply so transfer of the release agent doesn't bother me too much.
Cheers...Chris

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
chriscnf - 4 Years Ago
Hanaldo - 4 Years Ago
chriscnf - 4 Years Ago
chriscnf - 4 Years Ago
Hanaldo - 4 Years Ago
chriscnf - 4 Years Ago
Hanaldo - 4 Years Ago
chriscnf - 4 Years Ago
chriscnf - 4 Years Ago
Hanaldo - 4 Years Ago
chriscnf - 4 Years Ago
Hanaldo - 4 Years Ago
chriscnf - 4 Years Ago
Hanaldo - 4 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search