Group: Forum Members
Posts: 680,
Visits: 1.9K
|
Hi Marco,
Thank you for your post.
Your list of requirements for this casting resin is quite long and you might find it difficult to satisfy all of these criteria in a standard 2-part thermoset casting resin. Some if the properties you're after are more like those of a structual thermoformable plastic (injection moulding) and less like those of a typical casting resin. You will need to look into some quite specialist polyurethane vacuum casting resins, the like of which we don't currently supply. You'll need to cast them under vacuum (so in a vacuum casting machine) but if you're a university student I expect you'll have access to such a machine.
I'll PM you with some contact details of some people who might be able to help.
Best regards, Matt
Matt Statham Easy Composites / Carbon Mods - Technical Sales
|