Did anybody made a mould of a car part that had been ceramic coated ?
I got parts in that have ultra protect 9H ceramic coating on them and there this is a 1K product I dont know if the easylease wil work on this .


Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Do a test man, always do a test. If ever you are in doubt about compatibility, don't commit to anything without doing a small test and making sure it will work as planned.

It should be fine. These types of 1k coatings work in a very similar same way as chemical mould sealers and are moisture curing, and they can be remarkably tough - even tougher than regular 2k coatings. They are designed to be chemically resistant and very stable once cured and bonded - but there are so many of them out there, and they are not all made equally. Definitely do a test and confirm with your own parts and materials so you can be certain.
K.C.C
K.C.C
Supreme Being (577 reputation)Supreme Being (577 reputation)Supreme Being (577 reputation)Supreme Being (577 reputation)Supreme Being (577 reputation)Supreme Being (577 reputation)Supreme Being (577 reputation)Supreme Being (577 reputation)Supreme Being (577 reputation)
Group: Forum Members
Posts: 54, Visits: 117
Hanaldo - 11/11/2020 6:28:19 PM
Do a test man, always do a test. If ever you are in doubt about compatibility, don't commit to anything without doing a small test and making sure it will work as planned.

It should be fine. These types of 1k coatings work in a very similar same way as chemical mould sealers and are moisture curing, and they can be remarkably tough - even tougher than regular 2k coatings. They are designed to be chemically resistant and very stable once cured and bonded - but there are so many of them out there, and they are not all made equally. Definitely do a test and confirm with your own parts and materials so you can be certain.

ok thnx, wil do a little test with it. 