Hi, in general, when it is better to use one or another?
On my specific case, I need to bond stainless steel to carbon fiber panel.
Appearance is not important.
The bond has to resist pull force, pull shocks, salt water.
UV resistance is desired but the part could be coated for UV protection so no big deal.

Thanks
Massimiliano
Reply
Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
torsten Ker - 10/26/2020 11:39:25 PM
PS: just to be sure I would tape up the surouding area of where the steel is to be bonded to and key the bonding resin surface a bit with wire wool.

Thanks, what do you mean by tape up the surrounding area?
To add carbon at the edge of the steel?

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
mporta71 - 5 Years Ago
torstenker - 5 Years Ago
             Thanks It will be 316 L
mporta71 - 5 Years Ago
torstenker - 5 Years Ago
mporta71 - 5 Years Ago
Hanaldo - 5 Years Ago
mporta71 - 5 Years Ago
torstenker - 5 Years Ago
mporta71 - 5 Years Ago
Rosta Spicl - 5 Years Ago
                     Even if soric?
mporta71 - 5 Years Ago
Rosta Spicl - 5 Years Ago
torstenker - 5 Years Ago
Rosta Spicl - 5 Years Ago
torstenker - 5 Years Ago
torstenker - 5 Years Ago
mporta71 - 5 Years Ago
Hanaldo - 5 Years Ago
             Thank you.
mporta71 - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search