When purchasing s-2 fiberglass, are there any product descriptions which distinguish whether the fiberglass is drapable or not. I have some old 10 oz. s-2 glass purchased years ago that is extremely drapable. What I purchased recently is very rigid and would never conform to a contour. Is calling and asking the only way to know for sure?

Thanks...Alan
Reply
ahender
a
Supreme Being (382 reputation)Supreme Being (382 reputation)Supreme Being (382 reputation)Supreme Being (382 reputation)Supreme Being (382 reputation)Supreme Being (382 reputation)Supreme Being (382 reputation)Supreme Being (382 reputation)Supreme Being (382 reputation)
Group: Forum Members
Posts: 38, Visits: 300
ahender - 10/25/2020 3:05:14 PM
When purchasing s-2 fiberglass, are there any product descriptions which distinguish whether the fiberglass is drapable or not. I have some old 10 oz. s-2 glass purchased years ago that is extremely drapable. What I purchased recently is very rigid and would never conform to a contour. Is calling and asking the only way to know for sure?

Thanks...Alan

Found my answer.