I wouldn't advise thinning the epoxy with acetone, it is sometimes ok (although not great practice) to thin epoxies when you are using it to coat somthing in a very thin layer. With infusion though, the acetone will boil under vacuum and being a closed process the acetone will not be able to evapourate from the resin so it will have significant structural effects. By all means experiment with it (that's half of what composites is all about!) but I don't thing that you are likely to get the results that you are after, maybe some one else here ahs tried it and can shed some light on the results!
Paul Statham Easy Composites / Carbon Mods - Technical
|