Group: Forum Members
Posts: 59,
Visits: 278
|
Here in Europe 2K hardeners with Isocyanate production or import is banned since 2017 and now mostly phased out and unavailable. Try looking for Non-Isocyanate hardeners with acrylic car paint. I spray once or twice a month too,using a 3M mask with NOISH approved P100 (60921) filter in a well ventilated room
|