Hi there,
I am looking for a method or technique or just ideas for “spreading” carbon tow as it is being wound off a spool and onto a “sheet making” drum. I have seen a couple YouTube videos of this process at a distance in a commercial setting but you cannot tell what exact technique/mechanism is being used to spread and thin the tow. I expect it may be a combination of pressure with some form of combing device. Wondering if anyone on the forum has knowledge of how this is done?

Fasta
Fasta
Supreme Being (6.3K reputation)Supreme Being (6.3K reputation)Supreme Being (6.3K reputation)Supreme Being (6.3K reputation)Supreme Being (6.3K reputation)Supreme Being (6.3K reputation)Supreme Being (6.3K reputation)Supreme Being (6.3K reputation)Supreme Being (6.3K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
konaMike - 10/1/2020 3:30:46 AM
Hi there,
I am looking for a method or technique or just ideas for “spreading” carbon tow as it is being wound off a spool and onto a “sheet making” drum. I have seen a couple YouTube videos of this process at a distance in a commercial setting but you cannot tell what exact technique/mechanism is being used to spread and thin the tow. I expect it may be a combination of pressure with some form of combing device. Wondering if anyone on the forum has knowledge of how this is done?

I imagine the fibre is basically dragged over/around a round bar or edge with some pressure to force it flatter. 





konaMike
k
Supreme Being (128 reputation)Supreme Being (128 reputation)Supreme Being (128 reputation)Supreme Being (128 reputation)Supreme Being (128 reputation)Supreme Being (128 reputation)Supreme Being (128 reputation)Supreme Being (128 reputation)Supreme Being (128 reputation)
Group: Forum Members
Posts: 9, Visits: 27
Fasta - 10/5/2020 5:55:09 AM
konaMike - 10/1/2020 3:30:46 AM
Hi there,
I am looking for a method or technique or just ideas for “spreading” carbon tow as it is being wound off a spool and onto a “sheet making” drum. I have seen a couple YouTube videos of this process at a distance in a commercial setting but you cannot tell what exact technique/mechanism is being used to spread and thin the tow. I expect it may be a combination of pressure with some form of combing device. Wondering if anyone on the forum has knowledge of how this is done?

I imagine the fibre is basically dragged over/around a round bar or edge with some pressure to force it flatter. 

Yes, I have been experimenting along those lines. This technique works although it seems is difficult to get a consistent width. I may need to adjust the number and diameter of the cylinders in my test jig. Also, since my initial post I found a commerical post for an offshore company that produces 'spread tow'. They mentioned using air pressure to distribute the tow but there was no details or images....cheers/