I'm planning to build a bicycle frame using a mixture of Carbon tubes, fabric and aluminium.
I will need to bond the aluminium to the carbon but I'm not too sure how I would do that. And also I will need to join carbon tubes together. 

I don't know what I will need to buy to do all this. I want to use a 12k weave as the surface layer. What else will I need?
Joe
Joe
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
Hi, Titch.

Here's a link I found. It might help you decide which process to choose. I know its not purely "Tube Assembling", but the way he assembles his frame is just like putting tubes together.

http://www.youtube.com/user/TheProjectJunkie1/videos?sort=dd&view=u&page=2

Hope it will help.

 



 


    A $1000 electronic device will always protect a 10 cents fuse
Edited 13 Years Ago by Joe
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Haha have seen the videos of projectjunkie a week ago... I planned to make a bike too, but after seeing his video's with all the problems,time and money he put in his project, I was like "Nàh' let's find something else BigGrin

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




brummelisa
brummelisa
Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)
Group: Forum Members
Posts: 20, Visits: 144
I'm also planning to build a bike (tt frame that looks like Cervelo P5).

Sure, it's lot to do and think about, but it's fun Smile

Anyway, I have found some other links that may be nice to see

http://fairwheelbikes.com/forum/viewtopic.php?t=6655
http://fairwheelbikes.com/forum/viewtopic.php?f=6&t=7194
http://fairwheelbikes.com/forum/viewtopic.php?f=6&t=7602

/ Marcus
mhdghoul
mhdghoul
Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)
Group: Forum Members
Posts: 49, Visits: 113
i do 1 thing for sure i know it will be very strong in bonding 1st i bond the 2 parts with epoxy (the two mixture tubes ) i prefer alteco or abro or whatever , i just align the two parts and stick them with papertape and leave the parts where i want to put the epoxy not covered then i add epoxy to exactly look like small dots and leave it till its done , after that i take of the paper tape and see if it was aligned perfectly if not i break the spots and try again if it is good ( this process is to stick the two parts together aligned only Wink .

the next step is to mix resin with cf cut into very small pieces (usually use left over for that) and it will look like fiber putty then i add the caatalist to it and fill the area between the two parts , this will make it very stong and the next day i sand it with a grinder to the shape and when u finish the part it will not be something od cause its the same exact color and its cf at the end .

best regards mhd alghoul mhdghoul@hotmail.com youtube channel :atmospherejo link is http://www.youtube.com/user/atmospherejo?ob=0&feature=results_main
kylle
kylle
Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)
Group: Forum Members
Posts: 34, Visits: 101
brummelisa (28/02/2012)
I'm also planning to build a bike (tt frame that looks like Cervelo P5).

Sure, it's lot to do and think about, but it's fun Smile

Anyway, I have found some other links that may be nice to see

http://fairwheelbikes.com/forum/viewtopic.php?t=6655
http://fairwheelbikes.com/forum/viewtopic.php?f=6&t=7194
http://fairwheelbikes.com/forum/viewtopic.php?f=6&t=7602

/ Marcus


I tink that kind of frame "monocoque" style its triky but doable at home...
brummelisa
brummelisa
Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)
Group: Forum Members
Posts: 20, Visits: 144
Yes, it's tricky, but this is the result so far.
I wish I took more photos during the build, but I thought building was more fun than documentary it

The next stage is to wrap several layers of CF around the joints

http://www.talkcomposites.com/Uploads/Images/3ceaa843-13d7-4846-a12e-5462.jpg
Joe
Joe
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
Looks awesome. Good luck for the next steps Wink

 



 


    A $1000 electronic device will always protect a 10 cents fuse
kylle
kylle
Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)
Group: Forum Members
Posts: 34, Visits: 101
I sell Cervelo's for a living!!! and that's right on the spot! perfect!! 

can u show the mould of the top tube? did u do integrated headset? it's maybe the picture but it seems the chain line is a bit to short!!
brummelisa
brummelisa
Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)
Group: Forum Members
Posts: 20, Visits: 144
Thanks Kylle.

I can unfortunately not show the mould, since I didn't use any mould when I made it. I simply made plug for each part and wrapped CF around it.
Yes, I made integrated headset and that was really tough. The reason is not only that it had to be perfectly aligned, but the fork was tapered.
I used my headsets to act as a mould and mounted them on the fork so they were aligned.
It took several days and tries to make it perfect. Right now, the headtube looks a bit ugly on the outside, but I will put some nice layers at the end.

Since I don't have a P5 Smile around me I simply used a photo in Photoshop to measure all the measurements. 
I agree that the chain stay looks a bit short, but I think it was just the photo.
Here you see an earlier photo with the wheels.

http://www.talkcomposites.com/Uploads/Images/070a312d-8bdb-4694-a340-ec13.jpg
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search