	Group: Forum Members 	        
    Posts: 2.5K, 
    Visits: 28K 
    
 
          
		     | 
				                       
                 
                
                    
			            Any good structural epoxy will do very well. My pick would be Araldite 2015. 
  The difficulty with aluminium is it oxidises super quickly, like virtually instantly after you have prepped it. So you end up bonding to the oxide layer rather than the aluminium itself, and this always fails first. There are methods you can use to prep the ali to enhance the bond, but for most applications it isnt necessary.                
			            				
			                                 
                     
                                            
                         
                    
                  
             |