I can't think of anything designed for purpose. You could experiment with mixing a normal resin with fumed silica to make it more paste like. Certainly one to experiment with on a bit of scrap material to see if it has the desired properties. You can make it thicker with more silica, add strength with chopped fibres of glass or carbon and make it sandable (at some loss of strength) by adding glass bubbles. However as its a new use it is all down to experimenting to see if its adequate.