To be fair it looks more like a messy joint rather than a pinch or crease in the material. In which case, it is more of a cosmetic concern. Would theoretically be slightly weaker due to misalignment, but as Fasta pointed out it is likely to just be in the outer layer.
I wouldn't worry about it too much, to me what you can see there doesn't look like any concern structurally speaking. The bigger concern is probably more a case of 'if this is what their cosmetic outer layer looks like, what did they do internally'. But, it's probably fine.
|