Hi,

I have no experience with Carbon fibre and do not understand anything about it so need someone to rest my mind.

I have just bought a second hand bike and the carbon fibre frame looks distorted at parts (I’ve attached two videos).

Does this mean the carbon fibre isn’t genuine or is this just a poorly made frame?

Could it cause any problems in the long term?

Cheers,
Lewis
Reply
LEWISGH
L
Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)Junior Member (17 reputation)
Group: Forum Members
Posts: 2, Visits: 25
Hanaldo - 7/12/2020 5:13:21 AM
Can't see anything attached

Maybe the files too big, here's some pictures