I make a lot of carbon kevlar panels and parts for rally car and always have the same problem 
when trimming & drilling parts.

When I cut the finished part to size I always get a fluffy dry cloth frayed edge not a sharp clean edge 
like when I make carbon parts. Why is this.
Even if I drill a hole right in the middle of a part it has a frayed edge.

My process is hand lay up 1x Carbon Kevlar, 2x Diolen, 1x carbon kevlar using epoxy resin and then vac bag.

Any help appreciated.

taimur
t
Supreme Being (484 reputation)Supreme Being (484 reputation)Supreme Being (484 reputation)Supreme Being (484 reputation)Supreme Being (484 reputation)Supreme Being (484 reputation)Supreme Being (484 reputation)Supreme Being (484 reputation)Supreme Being (484 reputation)
Group: Forum Members
Posts: 32, Visits: 122
Add the picture please.

Dieseldave
D
Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)
Group: Forum Members
Posts: 7, Visits: 83
taimur - 6/16/2020 8:38:50 AM
Add the picture please.

No pictures I'm afraid as I'm working away from home at the minute.

Basically, it's a dry cloth edge that could be trimmed with a shears even though 
the part is made with gel coat and properly wet out with resin.

I make carbon parts in the same way but get a nice clean cut edge.

Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
You're using a material that is renowned for its abrasion resistance, and then surprised when it doesn't abrade cleanly... 
Dieseldave
D
Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)
Group: Forum Members
Posts: 7, Visits: 83
Hanaldo - 6/16/2020 1:12:31 PM
You're using a material that is renowned for its abrasion resistance, and then surprised when it doesn't abrade cleanly... 

So are you saying this is a normal finish for Kevlar?

Here are some pictures of what I am working on, I don't know the science behind the products etc I just 
put stuff in a mould.

[url=https://flic.kr/p/2jcpLKK]

[url=https://flic.kr/p/2jctPUB]

beliblisk
b
Supreme Being (813 reputation)Supreme Being (813 reputation)Supreme Being (813 reputation)Supreme Being (813 reputation)Supreme Being (813 reputation)Supreme Being (813 reputation)Supreme Being (813 reputation)Supreme Being (813 reputation)Supreme Being (813 reputation)
Group: Forum Members
Posts: 53, Visits: 2.8K
Cut with angel grinder and then use finer grids (at least 400) to wet sand it.


Dieseldave
D
Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)
Group: Forum Members
Posts: 7, Visits: 83
Thank you for the reply. I am currently cutting with a 1mm cutting disc in a 4.5" grinder.

Do you start with a 400 grit or work your way up from 80/120 etc?
beliblisk
b
Supreme Being (813 reputation)Supreme Being (813 reputation)Supreme Being (813 reputation)Supreme Being (813 reputation)Supreme Being (813 reputation)Supreme Being (813 reputation)Supreme Being (813 reputation)Supreme Being (813 reputation)Supreme Being (813 reputation)
Group: Forum Members
Posts: 53, Visits: 2.8K

Same cutting disc here. 1mm thick and i tend to use angel grinder for all but smallest cuts. 

I start with 400 wet for kevlar hybrids (for rough trim you can also use 320 sanding tools like Permagrid but it helps if you only work in one direction)  and i find that finishing edges with 800 is good enough in my bookSmile 

Coarse paper like 80/120 will leave exposed fibers hanging. 

Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You can sand them off as above or if you've just got a few stragglers left, you can use a fresh scalpel blade to cut them off. Its an unfortunate side effect of the abrasion resistance and cut resistance of kevlar and diolen so it is quite normal to have these issues.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Dieseldave
D
Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)Supreme Being (106 reputation)
Group: Forum Members
Posts: 7, Visits: 83
Many thanks for your help, Appreciate it.