Group: Forum Members
Posts: 7,
Visits: 83
|
I make a lot of carbon kevlar panels and parts for rally car and always have the same problem when trimming & drilling parts.
When I cut the finished part to size I always get a fluffy dry cloth frayed edge not a sharp clean edge like when I make carbon parts. Why is this. Even if I drill a hole right in the middle of a part it has a frayed edge.
My process is hand lay up 1x Carbon Kevlar, 2x Diolen, 1x carbon kevlar using epoxy resin and then vac bag.
Any help appreciated.
|