Hey guys i vacuum bagged CF , using gelcoat as first layer, then brush resin , put CF on resin, we out and bagged, its undercover for  bike, check the picture , there is unsaturated fiber, how do you think :


1. What was the reason of fail? what did wrong ?

2. Can I repair it now in anyway ?




This is how it look - I have few such places like this "hole"



http://www.compositescentral.com/attachment.php?attachmentid=2035&d=1354434807