What Vacuum Required?


Author
Message
dilligaf76
dilligaf76
Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)Supreme Being (520 reputation)
Group: Forum Members
Posts: 49, Visits: 115
Hi, can anyone tell me what the required Vacuum pressure is required for wet laying Carbon Fibre?
Replies
oekmont
oekmont
Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
When you do infusion, full vacuum is important. Otherwise there would be trapped air in every corner, because the resin would overflow the corner, leaving behind a cavity of 50% pressurised air. During the process the cavity will shrink down to half it's size while it reaches atmospheric pressure. Accordingly a 100% vacuum cavity shrinks down to zero size.
And you should remember that rotary vane pumps were not invented for composite use only, especially not for vacuum bagging. Many applications require a high vacuum, vacuum bagging does not.

Prepreg is produced in a way that there is not much air inside the resin itself. The vacuum will not degas the resin, but it helps to get air out of the system. The pressure inside the autoclave is for the last percents of performance. Out of autoclave prepreg works too, just not quite as good as regular prepreg in an autoclave.

Steve Broad
Steve Broad
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
oekmont - 6/12/2020 9:21:50 AM
When you do infusion, full vacuum is important. Otherwise there would be trapped air in every corner, because the resin would overflow the corner, leaving behind a cavity of 50% pressurised air. During the process the cavity will shrink down to half it's size while it reaches atmospheric pressure. Accordingly a 100% vacuum cavity shrinks down to zero size.
And you should remember that rotary vane pumps were not invented for composite use only, especially not for vacuum bagging. Many applications require a high vacuum, vacuum bagging does not.

Prepreg is produced in a way that there is not much air inside the resin itself. The vacuum will not degas the resin, but it helps to get air out of the system. The pressure inside the autoclave is for the last percents of performance. Out of autoclave prepreg works too, just not quite as good as regular prepreg in an autoclave.

Right, for infusion and prepreg the better the vacuum the better. For wet layup, not so important. Got it.

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
dilligaf76 - 5 Years Ago
Steve Broad - 5 Years Ago
dilligaf76 - 5 Years Ago
Steve Broad - 5 Years Ago
explorecomposites - 5 Years Ago
dilligaf76 - 5 Years Ago
Steve Broad - 5 Years Ago
taimur - 5 Years Ago
oekmont - 5 Years Ago
Steve Broad - 5 Years Ago
oekmont - 5 Years Ago
Steve Broad - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search