Would I be better with Prepreg ?


Author
Message
Damien
Damien
Supreme Being (293 reputation)Supreme Being (293 reputation)Supreme Being (293 reputation)Supreme Being (293 reputation)Supreme Being (293 reputation)Supreme Being (293 reputation)Supreme Being (293 reputation)Supreme Being (293 reputation)Supreme Being (293 reputation)
Group: Forum Members
Posts: 32, Visits: 132
OK...here is a part that I am making. Here is the mould. I did it with the EC gelcoat and paste for high temperature, anticipating that I could then use it for hand layup and prepreg. I am making my first part by hand layup (because I need to check all dimensions are good at the end). But man it was a mess with all the shapes...do you guys think that I would really be better with prepreg or would it be just as hard ?
Thanks !

Reply
Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Chris Rogers - 5/11/2020 1:20:43 AM
Massimiliano - 5/10/2020 4:25:52 AM
Chris Rogers - 5/5/2020 9:16:03 PM


Here's a video of the wet-preg method - not super helpful for a flat panel - but it's just to show the process:  https://youtu.be/06-0Vxs_9nY  

Hi, the link is not working... could you please repost it?
Thanks

Sorry - fixed it in the original post.  

Thank you!

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Damien - 5 Years Ago
Hanaldo - 5 Years Ago
Damien - 5 Years Ago
oekmont - 5 Years Ago
Damien - 5 Years Ago
oekmont - 5 Years Ago
Hanaldo - 5 Years Ago
explorecomposites - 5 Years Ago
Damien - 5 Years Ago
Hanaldo - 5 Years Ago
mporta71 - 5 Years Ago
             Sorry - fixed it in the original post.
explorecomposites - 5 Years Ago
                 Thank you!
mporta71 - 5 Years Ago
Damien - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search