Would I be better with Prepreg ?


Author
Message
Damien
Damien
Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)Supreme Being (295 reputation)
Group: Forum Members
Posts: 32, Visits: 132
OK...here is a part that I am making. Here is the mould. I did it with the EC gelcoat and paste for high temperature, anticipating that I could then use it for hand layup and prepreg. I am making my first part by hand layup (because I need to check all dimensions are good at the end). But man it was a mess with all the shapes...do you guys think that I would really be better with prepreg or would it be just as hard ?
Thanks !

Reply
oekmont
oekmont
Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
As I would consider it possible done with infusion, it should be possible with prepreg with the help of a heat gun. I would definitely not do it. I would cut out the middle bump for the first layer, and do it with a second piece with a 1cm overlap. The next layer than leaves out the 1cm overlap section. The third one again with overlap and so on. This looks like a small car interior part. 2mm would be way overengineered for that.

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Damien - 5 Years Ago
Hanaldo - 5 Years Ago
Damien - 5 Years Ago
oekmont - 5 Years Ago
Damien - 5 Years Ago
oekmont - 5 Years Ago
Hanaldo - 5 Years Ago
explorecomposites - 5 Years Ago
Damien - 5 Years Ago
Hanaldo - 5 Years Ago
mporta71 - 5 Years Ago
             Sorry - fixed it in the original post.
explorecomposites - 5 Years Ago
                 Thank you!
mporta71 - 5 Years Ago
Damien - 5 Years Ago