	Group: Forum Members 	        
    Posts: 19, 
    Visits: 84 
    
 
          
		     | 
				                       
                 
                
                    
			            I hope all is well with everyone!
  I finally managed to produce a usable Mold. Though, now that I reached this stage, what is the next best recommended move to ready the mold? Would I need to wet sand it, polish it, then add mold sealer and so on? (The mold was produced using Black Tooling Gelcoat)
  Any suggestions would be kindly appreciated. 
  Raf                
			            				
			                                 
                     
                                            
                         
                    
                  
             |