Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Mould Making
»
Mould reaction
Mould reaction
Post Reply
Like
3
Mould reaction
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Hansson43
H
Hansson43
posted 4 Years Ago
ANSWER
HOT
Topic Details
H
Group: Forum Members
Posts: 23,
Visits: 2.1K
Hi I recently made a mould from a front lip to a car in ABS-plastic and once I de-moulded it, it looked like the pictures. It's not that big of a deal I can fix it with some sandpaper. I just wonder though if you have any idea why this happened ? I found out afterwards that my Easylease went out of date by a a lot, could it be the easy lease being old ?
And the uni mould system I've use were also on the wrong side of the due date. But I tested the it befor application and it seemed alright.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Mould reaction
Hansson43
-
4 Years Ago
ABS is not easy to mould off. Not only does it deform at relatively low temperatures, but it is a bit vulnerable to styrene attack as well. Easylease or any other chemical release agent is not...
Hanaldo
-
4 Years Ago
Thank you so much for your answer Hanaldo! You are the man, Happy Easter
Hansson43
-
4 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search