Hi there,

I bought some 2nd hand carbon rimed (braking surface too) bicycle wheels from eBay. The front one is showing what I believe is some signs of age and impact damage. I'd like to attempt to repair these but have never worked with composites before. I'm thinking of getting some low viscosity resin, trying to inject into any cracks / gaps with a syringe, bag and clamp and then sand down with high grade of wet or dry. 

Does that sound like it might work to someone more experienced than me? I'd spotted the product linked below and wondered is that the best thing to use to attempt the repair with?

Any help or advice welcome, I've attached an image to this thread also so you can hopefully see the issues I'm trying to correct.

Thanks in advance.

https://www.easycomposites.co.uk/300g-22-twill-kevlar-cloth


Replies
kendokelso
k
Forum Guru (51 reputation)Forum Guru (51 reputation)Forum Guru (51 reputation)Forum Guru (51 reputation)Forum Guru (51 reputation)Forum Guru (51 reputation)Forum Guru (51 reputation)Forum Guru (51 reputation)Forum Guru (51 reputation)
Group: Forum Members
Posts: 4, Visits: 7
scottracing - 2/29/2020 10:05:20 PM
As lester has said repairing wheels in any way needs a high temp resin, as the friction area is always susceptible to delamination.

Just applying a resin  wont fix this problem it needs the carbon material removed and new plies applied and cured.This is possible but I certainly wouldn't use the wheel on the road unless you have used the correct materials.
https://carbonbikerepair.co.uk/#about

Is braking temp the main issue? Could I use them on a track bike or fixie after a poor to mediocre repair?

Lester Populaire
L
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
kendokelso - 3/1/2020 12:33:30 AM
scottracing - 2/29/2020 10:05:20 PM
As lester has said repairing wheels in any way needs a high temp resin, as the friction area is always susceptible to delamination.

Just applying a resin  wont fix this problem it needs the carbon material removed and new plies applied and cured.This is possible but I certainly wouldn't use the wheel on the road unless you have used the correct materials.
https://carbonbikerepair.co.uk/#about

Is braking temp the main issue? Could I use them on a track bike or fixie after a poor to mediocre repair?

Yes if is mainly about the brake surface. It is actually a pretty stupid use case for composites with the bad heat transfer and the limited temperatures they can handle, directly in the most stressed area. Imagine the tire rolling of the rim in a hairpin on a big descent. It's gonna result in a bad week...
For a track bike, fixie or with disc brakes i think you should be fine!

kendokelso
k
Forum Guru (51 reputation)Forum Guru (51 reputation)Forum Guru (51 reputation)Forum Guru (51 reputation)Forum Guru (51 reputation)Forum Guru (51 reputation)Forum Guru (51 reputation)Forum Guru (51 reputation)Forum Guru (51 reputation)
Group: Forum Members
Posts: 4, Visits: 7
Lester Populaire - 3/1/2020 9:06:16 AM
kendokelso - 3/1/2020 12:33:30 AM
scottracing - 2/29/2020 10:05:20 PM
As lester has said repairing wheels in any way needs a high temp resin, as the friction area is always susceptible to delamination.

Just applying a resin  wont fix this problem it needs the carbon material removed and new plies applied and cured.This is possible but I certainly wouldn't use the wheel on the road unless you have used the correct materials.
https://carbonbikerepair.co.uk/#about

Is braking temp the main issue? Could I use them on a track bike or fixie after a poor to mediocre repair?

Yes if is mainly about the brake surface. It is actually a pretty stupid use case for composites with the bad heat transfer and the limited temperatures they can handle, directly in the most stressed area. Imagine the tire rolling of the rim in a hairpin on a big descent. It's gonna result in a bad week...
For a track bike, fixie or with disc brakes i think you should be fine!

Thanks, that's all really interesting info. Good point about stupid use case. I prefer an alloy braking surface anyway, more feel and more progressive, carbon tends to be a bit "grabby". Totally right about tire coming off rim, gonna be a very bad week. Thankfully I live by the coast and have a selection of bikes, plus I don't ride fast or hard these days. 

So seems my options are:
1: Try and find this resin that is not made for prepreging and has a Tg high enough, do best repair I can, if successful then only use on flat roads and never aggressively, lots of rear brake (good rim). If not, bin wheels.
2: Start a little pet project track / single speed build, repair with a fairly standard low viscosity resin just to make use of these wheels. 
3: Continue the long search on eBay for a matching good condition front replacement.
4: Bin a nice carbon wheelset and cry myself to sleep ...

I do appreciate your comments and advice however, so thanks for taking the time. Just really don't want the answer to be option 4!

Edited 5 Years Ago by kendokelso
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
kendokelso - 5 Years Ago
SleepingAwake - 5 Years Ago
kendokelso - 5 Years Ago
Buchado - 5 Years Ago
scottracing - 5 Years Ago
kendokelso - 5 Years Ago
SleepingAwake - 5 Years Ago
kendokelso - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search