Cloudiness and white specks in finished project


Author
Message
SRTCobra
SRTCobra
Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)Junior Member (12 reputation)
Group: Forum Members
Posts: 2, Visits: 15
Hey guys!  I'm new to the forum, and new to composites in general.  My first project involved using a Red CF/Kevlar Fabric to hand lay up some side Moldings on my Jeep Grand Cherokee SRT8.  It took me a couple tries to figure out how to get it to stay tight on the part, and wait for the perfect time to lay down the cloth.  I finally got that down, and thought I was doing everything correctly.  Followed all instructions, advice, etc.  Anyway, after I got the finish perfectly smooth and scratch free, I looked at all four panels in the light and to my disgust, it was cloudy in the majority of places, with little white specks everywhere.  I don't know what I did wrong to get this cloudiness and specking.  It also looks like it goes all the way through to the CF weave.  I'm dumbfounded and don't even want to try again, if after all that hard work it's going to come out looking like this again.  I posted a picture of what I'm talking about.  It does not show the white specking, but you can see the cloudiness, especially towards the right.  And unfortunately this is not the worst one.  Any advice?
Thanks in advance,
Cody



White Specks

Edited 13 Years Ago by SRTCobra
Reply
charnwooduk
charnwooduk
Forum Guru (51 reputation)Forum Guru (51 reputation)Forum Guru (51 reputation)Forum Guru (51 reputation)Forum Guru (51 reputation)Forum Guru (51 reputation)Forum Guru (51 reputation)Forum Guru (51 reputation)Forum Guru (51 reputation)
Group: Forum Members
Posts: 7, Visits: 149
If I want to sand to a 1500 grit finish, then I go up in stages. 200grit > 400 grit >800 grit > 1200grit > 1500grit.

going from a very course grit directly to a very fine grit, you will find the fine grit is not agressive enough to sand down the deep scratches from 200 grit.