Depends on the resin system - the manufacturers data should give you the proper pot life etc.
You can degas the parts of the resin separately but you will add air to the mix when mixing so it would not be that beneficial.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|