I have my bonnet which in some places have paint come off.
If I use filler to cover level differences and flash tape on top should ok?
I plan tu use it to make a mould from it.
And rust spots I know Wink

Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Lester Populaire - 1/25/2020 6:22:48 AM
I honestly would just spray a 1k primer and then use a wax based release instead of pva. This won't dissolve the 1k primer and when demoulding in worst case you ripp off the two little primer patches off of the plug, but with a little acetone they will wash right off and leave you with a good surface otherwise. 

Unless the gelcoat attacks the areas of 1k primer, causing alligatoring in both. Then it's a lot of work to fix again. Fairly likely to happen. 

Classiccarbon, yes use any gun you like. PVA can cause it to rust out, so make sure you clean it out well if it is a gun you want to keep in good condition.

Also yes, you can use spray glue (though I'm not sure why you want to if you are making a mould?). Just be careful if you need to reposition anything after sticking it down, as you may lift the PVA film. It is normally ok though.

Classicarbon
C
Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)
Group: Forum Members
Posts: 86, Visits: 639
Hanaldo - 1/26/2020 5:32:58 PM
Lester Populaire - 1/25/2020 6:22:48 AM
I honestly would just spray a 1k primer and then use a wax based release instead of pva. This won't dissolve the 1k primer and when demoulding in worst case you ripp off the two little primer patches off of the plug, but with a little acetone they will wash right off and leave you with a good surface otherwise. 

Unless the gelcoat attacks the areas of 1k primer, causing alligatoring in both. Then it's a lot of work to fix again. Fairly likely to happen. 

Classiccarbon, yes use any gun you like. PVA can cause it to rust out, so make sure you clean it out well if it is a gun you want to keep in good condition.

Also yes, you can use spray glue (though I'm not sure why you want to if you are making a mould?). Just be careful if you need to reposition anything after sticking it down, as you may lift the PVA film. It is normally ok though.

Ah yes my mistake don't need glue haha. Thank you.

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Classicarbon - 5 Years Ago
Hanaldo - 5 Years Ago
Classicarbon - 5 Years Ago
Warren (Staff) - 5 Years Ago
Hanaldo - 5 Years Ago
Classicarbon - 5 Years Ago
Hanaldo - 5 Years Ago
Classicarbon - 5 Years Ago
Warren (Staff) - 5 Years Ago
SleepingAwake - 5 Years Ago
Hanaldo - 5 Years Ago
                 Ah yes my mistake don't need glue haha. Thank you.
Classicarbon - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search