I have my bonnet which in some places have paint come off.
If I use filler to cover level differences and flash tape on top should ok?
I plan tu use it to make a mould from it.
And rust spots I know Wink

Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yeh 2k high build primer. I would always then top coat that properly too, I don't like moulding off primer as it's very hit and miss. But your call.

Can also spray PVA release agent, quite reliable even on a 1k coating. But will take some refinishing to get the mould up to scratch.
Classicarbon
C
Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)
Group: Forum Members
Posts: 86, Visits: 639
Hanaldo - 1/21/2020 3:20:54 PM
Yeh 2k high build primer. I would always then top coat that properly too, I don't like moulding off primer as it's very hit and miss. But your call.

Can also spray PVA release agent, quite reliable even on a 1k coating. But will take some refinishing to get the mould up to scratch.

I Will struggle to use 2k Primer so might need to stay with flash tape and then smooth out the mould.

Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Classicarbon - 1/21/2020 3:53:21 PM
Hanaldo - 1/21/2020 3:20:54 PM
Yeh 2k high build primer. I would always then top coat that properly too, I don't like moulding off primer as it's very hit and miss. But your call.

Can also spray PVA release agent, quite reliable even on a 1k coating. But will take some refinishing to get the mould up to scratch.

I Will struggle to use 2k Primer so might need to stay with flash tape and then smooth out the mould.

It really is virtually impossible to get rid of flash tape marks without digging a massive low spot in the mould. Much better off using a 1k primer and just spraying PVA release agent as Warren said.

Classicarbon
C
Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)
Group: Forum Members
Posts: 86, Visits: 639
Hanaldo - 1/21/2020 3:20:54 PM
Yeh 2k high build primer. I would always then top coat that properly too, I don't like moulding off primer as it's very hit and miss. But your call.

Can also spray PVA release agent, quite reliable even on a 1k coating. But will take some refinishing to get the mould up to scratch.

Is that gun Will be enough Good for PVA ?
And can I apply  spray glue on top of it after?

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Classicarbon - 5 Years Ago
Hanaldo - 5 Years Ago
Classicarbon - 5 Years Ago
Warren (Staff) - 5 Years Ago
Hanaldo - 5 Years Ago
Classicarbon - 5 Years Ago
Hanaldo - 5 Years Ago
Classicarbon - 5 Years Ago
Warren (Staff) - 5 Years Ago
SleepingAwake - 5 Years Ago
Hanaldo - 5 Years Ago
                 Ah yes my mistake don't need glue haha. Thank you.