Hello, 

I'm part of a student design team looking to make kevlar enclosures from a negative mould. I've done work in the past with carbon fibre in an MDF mould, which I sealed with gelcoat. However, gelcoat was a huge pain to work with, didn't sand well, poor surface finish, etc.

This time I'm looking to use either aluminium or closed-cell polyurethane foam, which I will be machining on a CNC router. What sort of mould release agents should I use? Is just a wax and some PVA ok? Are there better mould materials to use? These are very low volume, room-temperature VARTM process moulds, 2-3 pulls max so I'm not concerned about long term durability, just ease of machinability and low price. The parts are also very small, largest is about 150x125x54mm. 

Thanks for your help!
Edited 5 Years Ago by JLiang
Reply
JLiang
J
Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)Forum Guru (52 reputation)
Group: Forum Members
Posts: 6, Visits: 57
Perfect. Thanks everyone for all your replies, much appreciated!
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
JLiang - 5 Years Ago
Hanaldo - 5 Years Ago
JLiang - 5 Years Ago
Hanaldo - 5 Years Ago
JLiang - 5 Years Ago
scottracing - 5 Years Ago
JLiang - 5 Years Ago
scottracing - 5 Years Ago
KLComposites - 5 Years Ago
JLiang - 5 Years Ago
explorecomposites - 5 Years Ago
allankn - 5 Years Ago
explorecomposites - 5 Years Ago
JLiang - 5 Years Ago
Hanaldo - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search