Aluminium must be much cheaper in the UK/US. I got a quote to have a 300x125 mould machined here, and local suppliers wanted AU$500 just for the billet and another $700 to machine it. I bought a 1500x500x50 block of PU tooling board for $275 and machined it myself...
|