Hi

I am currently building a Datsun 240Z and wanted to make some of the parts from carbon fibre. The body shop repaired all of the body parts, sanded them and primiered them ready to be painted.
This is how it is now. 

So that the mold won't stick to the primer what is the best thing to do? Do I have to paint the parts or atleast clearcoat them?



Reply
Lester Populaire
L
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
4age - 12/31/2019 3:39:32 PM
Hi

Wow you guys are very quick!

So basically if i just wax the 2K primered body parts and use easyeasy lease, there should be little risk of the fiberglass mold sticking to the 2k primered steel parts?

Thanks for your help !

This are my first complex parts.  Until know I just made same small carbon patches on a sheet of glass, for sending them to get tested for street aproval.

I always recommend to make a small scale test if you are working with materials and or processes you are not familiar with.  It will save you time and headaches in the long run, especially on a big process like this!
Other than that make sure to keep us posted! I'm not a car guy but love the 240Z from street bandito so this will be a good one!

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
4age - 6 Years Ago
K.C.C - 6 Years Ago
SleepingAwake - 6 Years Ago
4age - 6 Years Ago
SleepingAwake - 5 Years Ago
f1rob - 5 Years Ago
4age - 5 Years Ago
Cliff Pountney - 5 Years Ago
Hanaldo - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search