I'm not sure if this is the correct place for this post as it covers several areas but here it goes. . . So a bit of background. . .
I've been working with fibreglass for 5 or 6 years now, mostly on a part time basis, making mainly body kits for drift cars as well as some parts for lorries. Along with the guy I work with, we are self taught by mainly trial and error, having been initially a car body repair shop to now solely fibreglass body kits. I use a hand layup process only and having read a few posts on here I believe I use polyester resin. It may seem odd to you to think I don't know what type of resin I use but until I came here I didn't realize there was any different types! Now I would like to move on my own and so as not to 'step on my friends toes' I've decided to try and work mainly with carbon fibre. So while I believe I have a good grasp of how fibreglassing works, it seems there is so much I don't know. The types of products I will be making will range from small items like wing mirror covers to more complicated items like doors bonnets and boot lids. Also I should mention I will still be working on a part time basis as I have a full time unrelated job. My intention is to put any money I make straight back in and try to make a successful business out of it. So a couple of questions.

1. What products do you think I would need to set myself up.
2. Would £1000 be a realistic starting point (I'm starting completely from scratch)
3. Would it be worth my while to take a course on CF as I have no experience with it or should I wing it as I have been doing all along!

Look forward to hearing from anyone. Thanks, David

This post gets a little messy after this. . . Problems with my cursor on iPad lol





Having watched your tutorial videos I believe resin infusion is the way to go.



4. 
Reply
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi David,

Thanks for the post and sorry for the delay in getting back to you. You're like-minded with many other customers both on this forum and that we deal with just through the business; we'd be very pleased to work with you and help you to grow your business (and ours too) by helping wherever we can.

It's tricky to know exactly what to tell you to spend your money on in terms of a start-up and, in many cases, not specialising in the beginning would mean that you would need more equipment and more types of material which pushes the startup costs up. For example, the best materials and equipment for making small details parts (like wing mirror covers) are different from the best materials and equipment for making larger parts (like bonnets). In this example, I would be thinking of pre-preg for the small parts and resin infusion for the larger parts. You can resin infuse small parts and you can pre-preg large ones but the most time and cost effective way to do each of those is those respective techniques.

Also, the standard you want to work to will have an impact. If you want to make completely professional parts you need to expect some hiccups during the learning curve (which will need to paid for!), and some decent equipment. We go pretty over the top in our videos in terms of using the best of everything but even working on a slightly stripped back version of making our carbon fibre bonnet you would be looking at more like £1800 by the time you'd bought the mould materials, all the equipment and the materials for the bonnet.

It might be worth deciding what your first parts will be and focussing on getting the equipment and materials you need for that first product. In this case, £1000 startup is probably perectly realistic. OK, you won't be a fully fledged composites company but if you specialise in a certain type of part then you could get up and running with that to get yourself going and then, as you say, put money back in to grow the business.

3. Would it be worth my while to take a course on CF as I have no experience with it or should I wing it as I have been doing all along!


This is totally up to you. I think everyone on this forum would agree (from doing things the hard way) that money spent on a course would pay for itself in terms of money not spent on wasted material and you move down the learning curve yourself. We sell materials and (now) courses so I can be impartial on it and say it really depends on what you prefer. Our resin infusion course for example is a 1 day course and at the end of it I can say with 100% confidence that you could resin infuse parts to a professional standard without any issues. Learning on a course would certianly be a quicker way to perfect a process such as this but it's by no means the only way.

I hope this helps and look forward to working with you.

All the best, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search