I'm going to make some wet lay moulds by hand using the EG160 tooling gel, EL160 resin and 450g carbon. I wanted to bag the moulds over night while the resin cures but want to know if regulating the vacuum is necessary? Does anyone have experience of using a regulator with hand laminating?
These moulds will be used to make parts in an autoclave. Obviously, tooling prepreg is available but the original part can't really be exposed to heat or pressure.
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Number of issues here:

1. Vacuum bagging moulds is totally pointless. Wet-lay vacuum bagging does not reduce void content, which is the primary concern for building moulds. Resin infusion and pre-preg are different stories, but vac bagging is purely done to increase the strength to weight ratio of the component, which generally speaking isn't a concern when building a mould. It doesn't matter if a mould is a bit heavy and resin rich, you aren't normally concerned about the weight.

2. I highly doubt the finished moulds will be suitable for autoclave use, EC may correct me here on the EG160, but composite moulds generally are not. You can get some toughened tooling pre-pregs that can be used in an autoclave, but wet-laid moulds with a gelcoat will very likely suffer under the combination of heat and pressure. 

3. The combination of fibreglass and carbon in a mould intended for pre-preg use can be troublesome. The different CTE between the two materials can cause lots of issues with warping and distortion.