Hi,

I've recently come on to a problem  of which I'd like to know the exact cause, so what better place to ask than here..

I've skinned a few  plastic parts in CF  using the black basecoat & EL epoxy (fast hardener) and everything went as usual .. perfect

I applied an automotive UV resistant clearcoat (by spraygun) and the parts all looked stunning.

Now after a couple of days on the car, we're starting to see and feel  "ribbels" form  that run along exactly with the carbon fibre weave.
I've spoken to a few other people here that are into skinning and all have had the same problem with some parts but cannot explain the cause. They all say  that sanding & re-clearing the part solves the problem, but I'd like to know what causes it.

Some parts were installed on cars that were in the sun, others were  in a garage and have seen no sun .. yet both suffer the same issue

Reply
Whitesol
Whitesol
Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)
Group: Forum Members
Posts: 7, Visits: 15
I usually allow at least a 24 hr curing time before sanding and a 48hr or longer gap between the last wetsand and the applying of the clearcoat, to prevent the risk of any moisture still being present.
I've re-cleared these specific parts  and they've been out in the sun  for a full day  allready with no sign of deforming again, so the problem does seem solved :-)