What's the material for making flanges in split moulds?

polypropylene, fluted correx, mdf, ....?
Reply
Warren
Warren
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Administrators
Posts: 214, Visits: 782
corex fluted signboard is perfect.

Cardboard is fine too when covered in flash breaker tape or a cheap parcel tape you know resin doesnt stick too.