Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Without degassing, it can be difficult to get the air out the brick underside. You will have to pour it in stages. Sometimes poking with a cocktail stick helps. Pouring the resin just over the brick, then gently wafting with a heat gun can be enough to make it sink into the brick voids.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|