GSX-R 600 fuel tank cover/protector vacuum infused. Pictures!


Author
Message
Legoman
Legoman
Supreme Being (467 reputation)Supreme Being (467 reputation)Supreme Being (467 reputation)Supreme Being (467 reputation)Supreme Being (467 reputation)Supreme Being (467 reputation)Supreme Being (467 reputation)Supreme Being (467 reputation)Supreme Being (467 reputation)
Group: Forum Members
Posts: 29, Visits: 622
Some thicker part designed for protection not just cosmetic purposes. 
200g twill
300g +-45° biaxial carbon fabric
400g +-45° biaxial carbon fabric
Honestly I didnt pay to much attention for the fiber orientation...next time.
Trimmed some different shape, and added basalt fibre on the side panel insted of carbon

GO