Will epoxy resin cure in a sealed container?


Author
Message
Mark Cooper
Mark Cooper
Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)
Group: Forum Members
Posts: 3, Visits: 12
Hi everyone. Newb resin user here. 
My workshop is dusty. Very dusty. If I pour my resin into moulds and then seal them inside containers (like Really Useful tubs) will they cure? Does the curing process need "air flow" or space for escaping gases?
Warren (Staff)
Warren (Staff)
Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The epoxy will cure even in a sealed tub as it is a Part A and Part B reaction where no air is needed just the relevant chemical components. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Mark Cooper
Mark Cooper
Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)
Group: Forum Members
Posts: 3, Visits: 12
Warren (Staff) - 7/17/2019 4:33:51 PM
The epoxy will cure even in a sealed tub as it is a Part A and Part B reaction where no air is needed just the relevant chemical components. 

Perfect, thanks :-)