Hi

I'm going to be making a mold of the part detailed below:

http://www.talkcomposites.com/3221/Looking-for-best-way-to-make-this-mould

I've used Epoxy tooling gel coat backed with polyester resin and CSM before and it's worked well for me.

can you suggest any alternatives?

The mold will be made in two parts and is intended to be used multiple times for carbon/epoxy parts using the vacuum bagging technique.

How much tooling gelcoat do  you think i would need?

Thanks in advance
Replies
Bonobo
Bonobo
Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)Supreme Being (711 reputation)
Group: Forum Members
Posts: 85, Visits: 1.2K
Thanks for the quick reply!

I think i'll be going with the uni-mold tooling gelcoat and backing up with polyester resin and CSM.

Still some work to go on the plug but I'll be finishing it in a 2k primer filler, do you think this will release ok once polished and waxed?
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Yes, that should be fine for a release. Give the paint a good bake (or lots of time) to fully cure, afetr that, I wouldn't expect any problems.

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search